Non-leafing Metallic Ipa Aluminiomu Pigment Powder | Aluminiomu Powder
Apejuwe:
Aluminiomu Pigment Powder, ti a mọ ni “iyẹfun fadaka”, ie awọ fadaka fadaka, ni a ṣe nipasẹ fifi iye kekere ti epo kun si bankanje aluminiomu mimọ, fifun parẹ sinu iyẹfun iwọn-iwọn nipasẹ lilu ati didan rẹ. Aluminiomu Pigment Powder jẹ ina, pẹlu agbara ewe giga, agbara ibora ti o lagbara, ati iṣẹ afihan ti o dara si ina ati ooru. Lẹhin itọju, o tun le di ti kii-leafing aluminiomu Pigment Powder. Aluminiomu Pigment lulú le ṣee lo lati ṣe idanimọ awọn ika ọwọ, ṣugbọn tun lati ṣe awọn iṣẹ ina. O tun le ṣee lo fun gbogbo iru awọn ti a bo lulú, alawọ, inki, alawọ tabi hihun, ati be be lo. Aluminiomu Pigment Powder jẹ ẹya nla ti awọn pigments ti fadaka nitori lilo jakejado rẹ, ibeere giga ati ọpọlọpọ awọn oriṣiriṣi.
Awọn abuda:
Aluminiomu pigment lulú ni awọn patikulu apẹrẹ flake. Awọn patikulu leefofo loju omi ni oju ti awọn aṣọ ti o pari, ti o ṣẹda apata si awọn gaasi ipata ati awọn olomi, o pese lilọsiwaju ati dada iwapọ ti awọn nkan ti a bo. Aluminiomu pigmenti pẹlu ohun elo ti agbara oju ojo to lagbara le farada ipata igba pipẹ ti ina oorun, gaasi ati ojo, nitorinaa o pese aabo to dara julọ si awọn aṣọ.
Ohun elo:
Ni akọkọ ti a lo ni ọpọlọpọ awọn ti a bo lulú, masterbatches, awọn aṣọ, inki, alawọ ati bẹbẹ lọ, lo si awọn aṣọ ita gbangba.
Ni pato:
Ipele | Akoonu ti kii ṣe iyipada (± 2%) | Iye D50 (μm) | Ajẹkù Sieve (44μm) ≤% | dada Itoju |
LP0210 | 95 | 10 | 0.3 | SiO2 |
LP0212 | 95 | 12 | 0.3 | SiO2 |
LP0212B | 95 | 12 | 0.3 | SiO2 |
LP0215 | 95 | 15 | 0.5 | SiO2 |
LP0218 | 95 | 18 | 0.5 | SiO2 |
LP0313 | 96 | 13 | 0.3 | SiO2 |
LP0316 | 96 | 16 | 0.5 | SiO2 |
LP0328 | 96 | 28 | 1 | SiO2 |
LP0342 | 96 | 42 | 1 (124μm) | SiO2 |
LP0354 | 96 | 54 | 1 (124μm) | SiO2 |
LP0618 | 96 | 18 | 0.5 | SiO2 |
LP0630 | 96 | 30 | 1 | SiO2 |
LP0638 | 96 | 38 | 1(60μm) | SiO2 |
LP0648 | 96 | 48 | 1 (124μm) | SiO2 |
LP0655 | 96 | 55 | 1 (124μm) | SiO2 |
Awọn akọsilẹ:
1.Jọwọ idanwo didara ọja ṣaaju lilo.
2.Avoid eyikeyi awọn ipo ti yoo da duro tabi leefofo lulú patikulu ni air, pa kuro lati ga otutu, ina nigba lilo ilana.
3.Tighten awọn ilu ti n lu ideri ọja ni kete lẹhin lilo rẹ, iwọn otutu ipamọ yẹ ki o wa ni 15 ℃- 35 ℃.
4.Store ni itura, ventilated, gbẹ ibi.Lẹhin igba ipamọ igba pipẹ, didara pigment le yipada, jọwọ tun ṣe idanwo ṣaaju lilo.
Awọn ọna pajawiri:
1.Lọgan ti ina kan ba jade, jọwọ lo erupẹ kemikali tabi awọn iyanrin ti o ni ina lati fi jade.Ko si omi ti o yẹ ki o lo lati pa ina naa.
2.Ti pigmenti ba wọ oju nipasẹ ijamba , o yẹ ki o wẹ wọn pẹlu omi mimọ fun o kere 15minutes ati ki o yipada si dokita fun ijumọsọrọ ni akoko.
Itọju egbin:
Iwọn kekere ti pigmenti aluminiomu asonu le jẹ sisun ni aaye ailewu nikan ati labẹ abojuto awọn eniyan ti a fun ni aṣẹ.